Cookie preferences
This website uses cookies, which are necessary for the technical operation of the website and are always set. Other cookies, which increase the comfort when using this website, are used for direct advertising or to facilitate interaction with other websites and social networks, are only set with your consent.
Configuration
Technically required
These cookies are necessary for the basic functions of the shop.
"Allow all cookies" cookie
"Decline all cookies" cookie
CSRF token
Cookie preferences
Currency change
Customer recognition
Customer-specific caching
Individual prices
PayPal payments
Selected shop
Session
Comfort functions
These cookies are used to make the shopping experience even more appealing, for example for the recognition of the visitor.
Note
Statistics & Tracking
Affiliate program
Facebook Pixel
Google Analytics
Google Analytics / AdWords
Track device being used
€37.01 inkl. MwSt.
€31.10 ohne MwSt.
€31.10 ohne MwSt.
Content: 0.05 Liter (€740.20 * / 1 Liter)
Prices incl. VAT plus shipping costs
Ready to ship today,
Delivery time appr. 1-3 workdays
- Order number: BMG-077-TG-
PRODUCT PRESENTATION - GOLD ELECTROLYTE 999 FINE GOLD - 23,8 CARAT ... more
Product information "Gold Solution 4 Gramm /Liter"
PRODUCT PRESENTATION - GOLD ELECTROLYTE 999 FINE GOLD - 23,8 CARAT
WITH 4 GRAMS OF GOLD PER LITER
Do-it-yourself gold plating has never been so easy. Our Gold Electrolyte from Betzmann Galvanik can be purchased by anyone. Whether it is for use in highly professional laboratories, industry, luxury companies, to the use in the hobby, main or secondary trade, companies, schools, universities, TH , IHK or other authorities.
With this extremely fast and very hard depositing gold electrolyte from Betzmann Galvanik, you can usually coat the following metals directly:
Stainless steel of all kinds, surgical steel, copper, silver, brass, nickel, iron, steel,
The pink color of the electrolyte is the hardness additive cobalt. This gives the otherwise much too soft gold an abrasion resistant surface. This is not toxic in the admixed composition.
The gold electrolyte from Betzmann Galvanik is anti-allergenic, was extracted from crisis- and conflict-free gold and is food-safe.
Our Betzmann Galvanik Gold Electrolyte has a very fast deposition and further achieves a very hard gold layer. It has a very good covering effect and is therefore one of the best products on the market worldwide. A special preservative results in a very long shelf life of at least 2 years and prevents sedimentation, which occurs with many other gold electrolytes.
The Gold Electrolyte from Betzmann Galvanik can be used for pen electroplating, pad electroplating and also for bath electroplating!
The Gold Electrolyte from Betzmann Galvanik is used worldwide, e.g. for the gold plating of boat parts made of brass that are exposed to salt water, medical technology, measurement technology, for optical gold plating, for technical gold plating, gold plating of drive shafts, musical instruments and their parts, both inside and outside, body jewelry, intimate protection, dental jewelry, dental technology, drills of all kinds, shisa, e-cigarettes so-called. Vaporizers, vehicle parts, engine parts, motorcycle parts, airplane interiors, exhaust systems and manifolds, as gold is very heat resistant, sporting goods, diving equipment, keys and pendants, jewelry, chains and rings of all kinds, piston rods, pipes, table feet, bathroom fixtures and many more.
Partial coatings are possible by masking and masking surrounding areas.
To avoid material loss when coating sloping surfaces, we recommend our thickener/gel former. With this you can thicken all electrolytes also chrome remover, cleaner etc..
Also you can use with this gold mostly in the ratio 1:10 our mixer products like rose gold, white gold and green gold!
Optimal results are achieved with the platinum electrode 6mm - 10cm long or the flat platinum electrode, since platinum electrodes can build up very thick layers far above 10 microns and more.
Graphite electrodes can also be used.
Gold content: 4 grams per liter
The procedure for gold plating:
It is recommended to polish the surface to a shine first - the nicer the surface, the nicer the shine will be
Thorough degreasing with the electrocleaner
Activate the surface with the activator
Gilding with platinum electrode starting around 5 volts
Operating Conditions and Deposit Data
Plating Factor | 0.01 A/cm2 |
Plating rate | 0.12 micron per minute at 0.01A/cm2 |
Maximum plating thickness | 4 microns |
Temperature | 18 – 25 °C |
pH | 4.4 – 5.0 |
Gold concentration | 4 grams per litre |
Agitation | Low |
Electrode | Mesh or Platinum Rod Electrode |
Gold content in plate | 99.9% (balance carbon) |
Cathode efficiency | ~25% at Plating Factor = 0.01A/cm2 |
Hardness | 190 – 210 Hv |
Density of deposit | 19.3 g/cm3 |
Stress | Medium |
Special storage requirements | Away from sunlight |
Shelf life | 1 – 2 years |
Health and Safety classification | Harmful |
Special considerations | Contains potassium cyanide (0.15%) |
Transport (UN number) | None: Not classified as dangerous for transport |

Signalword: Warning
H-phrases:
H332 Harmful by inhalation.
H312 Harmful in contact with skin.
H302 Harmful if swallowed.
EUH032 Contact with acids liberates very toxic gas.
P phrases:
P280 Wear protective gloves/protective clothing/eye protection/face protection.
P301 IF INSPECTED:P310 Immediately call a POISON CENTER/doctor.
Related links to "Gold Solution 4 Gramm /Liter"
Available downloads:
Read, write and discuss reviews... more
Customer evaluation for "Gold Solution 4 Gramm /Liter"
Write an evaluation
Evaluations will be activated after verification.
Viewed